Induction Brazing carbide teeth to steel pipe
Views Send Enquiry
Objective Brazing carbide teeth to a steel jaw in less than 5 minutes
Material Steel pipe jaw, 0.5” (12.7mm) dia, 1.25” (31.75mm) long, 0.25” (6.35mm) thick carbide teeth, black flux and silver copper braze shims
Temperature 1292ºF (700ºC)
Frequency 257kHz
Equipment • Power of 6 kW induction heating system, equipped with a remote workhead containing one 0.66μF capacitor
• An induction heating coil designed and developed specifically for this application.
Process A two turn rectangular helical coil is used to heat the carbide and steel to 1292ºF (700ºC) for 4 to 5 minutes. Three braze shims control the amount of braze and the even heat allows for a good flow of braze creating an aesthetically pleasing bond.
Results/Benefits Induction heating provides:
• Hands-free heating that involves no operator skill for manufacturing
• Consistent, repeatable aesthetically pleasing brazes
• Even distribution of heating

Brazing carbide teeth to steel pipe
Related Content

Air Cooled clamp coil (half-open coil) for preheating gas pipeline

induction coating by air cooled clamp induction coil

Remove plastic coating from steel tubes by Induction Heating

Releasing Fixture by Induction Heating

U shape air cooled induction coil by UM-100C-HF for pipeline preheating

induction quenching with custom-design inductor

induction brazing diamond segment

induction brass soldering copper plate_2










Newest Comment
No Comment
Post Comment