Induction Brazing Steel Conduit
Views Send Enquiry
   Objective To heat a stainless steel conduit, ferrule and elbow assembly to 1400°F (760°C) within 20 seconds for brazing.
  Material 6”(152.4mm)long x 0.5”(12.7mm) diameter stainless steel conduit, 0.5”(12.7mm) long x 0.5”(12.7mm) diameter ferrule, 2”(50.8mm) elbow with 0.5” (12.7mm) diameter
  Temperature 1400°F (760°C)
  Frequency 70 kHz
  Equipment •  Power of 15 kW induction heating system equipped with a remote workhead
  • An induction heating coil designed and developed specifically for this application.
  Process A specially designed, three-turn helical coil is used to provide heat to the assembly at the braze joint area. Two small silver solder braze rings are placed at each joint; the joints are coated with black flux to insure that the braze material flows cleanly. The assembly is placed inside the coil and power is applied for 15 seconds to cause the braze to flow.
  Results/Benefits Induction heating provides:
  • Consistent and repeatable results
  • No flame process
  • Faster process time  
   
  brazing-steel-Ferrule  
Related Content
 - Air Cooled clamp coil (half-open coil) for preheating gas pipeline
 - induction coating by air cooled clamp induction coil
 - Remove plastic coating from steel tubes by Induction Heating
 - Releasing Fixture by Induction Heating
 - U shape air cooled induction coil by UM-100C-HF for pipeline preheating
 - induction quenching with custom-design inductor
 - induction brazing diamond segment
 - induction brass soldering copper plate_2










Newest Comment
No Comment
Post Comment