Induction Shrink fit steel gear
Views Send Enquiry
Objective Heat the bore of a hardened spur steel gear to shrink fit onto a gear motor shaft. This is part of a chair for the disabled.
Material Steel gear 2.5″ h (63.5mm) OD, .75″ h (19mm) ID x .625″ h (16mm) thick, temperature indicating paint
Temperature 400 oF (204 oC)
Frequency 30 kHz
Equipment .Power of 15 kW induction heating system, equipped with a remote workhead containing two 0.66 ƒÊF capacitors for a total of 1.32 ƒÊF
. An induction heating coil designed and developed specifically for this application.
Process A four turn helical internal coil is used to heat the gear bore. The coil is inserted into the gear bore and power is applied for 10 seconds to reach the required 400 oF (204 oC) and expand the gear bore. The gear is then placed on the shaft and allowed to cool, creating the shrink fit between the gear and the shaft.
Results/Benefits Induction heating provides:
. No pre-heat cycle, heat is available on demand
. Energy efficient, heats only the part, not the atmosphere around it
. Controlled, even distribution of heating
. Faster production times

shrink fit steel gear
Related Content

Air Cooled clamp coil (half-open coil) for preheating gas pipeline

induction coating by air cooled clamp induction coil

Remove plastic coating from steel tubes by Induction Heating

Releasing Fixture by Induction Heating

U shape air cooled induction coil by UM-100C-HF for pipeline preheating

induction quenching with custom-design inductor

induction brazing diamond segment

induction brass soldering copper plate_2
Hot

induction shrink fitting motor (stator or rotor)
induction installation (shrink fitting) couplings for Shaft Collar with flexible induction coil
induction shrink fitting wheel
induction shrink fitting stator
induction shrink fitting spindle
induction shrink fitting for rotor and stator
air cooled induction heating for fixing Nuclear Power Unit (loosen screw nut)
induction shrink fitting

Newest Comment
No Comment
Post Comment