Induction Soldering fabric to kovar tip
Views Send Enquiry
Material Kovar cone, base 3/8” (9.5mm) dia, cone 3/8” (9.5mm) high, solder
Temperature 300 ºF (149 ºC)
Frequency 242 kHz
Equipment • Power of 3.2 kW induction heating system, equipped with a remote workhead containing one 1.2μF capacitor.
• An induction heating coil designed and developed specifically for this application.
Process A three turn pancake coil is used to heat the tip of the cone to 300 ºF (149 ºC) in 2-3 seconds. The coil design allows for easy placement of the fiber across the tip of the cone and reduces the heat flow to the bottom of the assembly for the manufacturing process.
Results/Benefits Induction heating provides:
• Hands-free heating that involves minimal operator skill for manufacturing.
• Precise, even heating.
• Repeatable, non-contact clean heat .

Soldering fabric to kovar tip
Related Content

Air Cooled clamp coil (half-open coil) for preheating gas pipeline

induction coating by air cooled clamp induction coil

Remove plastic coating from steel tubes by Induction Heating

Releasing Fixture by Induction Heating

U shape air cooled induction coil by UM-100C-HF for pipeline preheating

induction quenching with custom-design inductor

induction brazing diamond segment

induction brass soldering copper plate_2









Newest Comment
No Comment
Post Comment