induction shrink fit steel gear
Shrink fit steel gear Objective Heat the bore of a hardened spur steel gear to shrink fit onto a gear motor shaft. This is part of a chair for the disabled.Material Steel gear 2.5 h (63.5mm) OD, .75 h (19mm) ID x .625 h (16mm) thick, temperature indicating…
-
induction shrink fitting carbide ring
Shrink fitting carbide ring Objective Shrink fitting a carbide ring into a steel valve seatMaterial Steel valve seat 6” (152.4mm) OD with 3” (76.2mm) ID hole & .75” (19mm) thick, carbide ringTemperature 500 F ( 260 C)Frequency 55 kHzEquipment • Pow…
-
induction shrink fitting impeller blades to shaft
Shrink fitting impeller blades to shaft Objective Heat aluminum impeller blades to 200 F (93 C) and shrink fit onto a shaft.Material Aluminum impeller blades with a .28” (7.109mm) bore, aluminum shaftTemperature 200 F (93 C)Frequency 255 kHzEquipment • P…
-
induction shrink fitting pulley to insert bearing
Shrink fitting pulley to insert bearing Objective Heat aluminum pulley for insertion of an inner bearing for the automotive industryMaterial Aluminum pulley 2.3” (60mm) OD x 1.6” (40mm) ID x 1” (27mm) high and inner bearing 0.7” (17.8mm) high x 1.6” (…
-
induction shrink fitting wrist pin into connecting rod
Shrink fitting wrist pin into connecting rod Objective Assemble connecting rods with a more accurate control of the heatMaterial Rod has an OD of .9125” (23.18mm), knuckle has an ID of .9125” (23.18mm) with an interference of .0001” (.0025mm). Knuckle a…
-
induction shrink fit camshaft gear
Shrink Fit Camshaft Gear Objective: Heating a camshaft gear with a bore size of 1.630 to shrink fit over a steel shaft that has a diameter of 1.632. A temperature of 5000F is required for the gear to expand 0.002 in order to slip over the shaft. Production…
-
induction soldering steel connectors
Soldering Steel Connectors Objective Heat an assembly of small, gold-plated steel connectors to a brass block. Material Approx. 1/8” (3.2mm) diameter gold-plated steel connectors, 1”(25.4mm) square x 1/4” thick brass block Temperature 600F(315.6C)…
-
induction soldering radio antenna
Soldering Radio Antenna Objective To heat a coaxial antenna assembly to 600F within 2 seconds for a soldering application. The goal to improve on an existing procedure with a soldering iron which required 10 to 15 seconds. Material .250” diameter alu…
-
induction solder flex circuits
Solder Flex Circuits Objective To heat multiple joints on flex circuit strips to 180-200F within seven seconds for a soldering application.Material Copper bonded to polyester flex circuit strips, Solder Plus Paste 63NC-A, 0.0625” thick Teflon sheetsTemper…
-
induction heating steel dogbone specimen
Heating Steel Dogbone Specimen Objective: To heat a magnetic steel dogbone specimen to 12000F as quickly as possible and sustained for tensile testing. Heating should take place using a helical coil placed square in relation to the long axis of the gage ar…