                            induction brazing steel conduit
                            
                              Objective To heat a stainless steel conduit, ferrule and elbow assembly to 1400F (760C) within 20 seconds for brazing. Material 6”(152.4mm)long x 0.5”(12.7mm) diameter stainless steel conduit, 0.5”(12.7mm) long x 0.5”(12.7mm) diameter ferrule, 2”(50.… 
- 
                            induction annealing steel tubes
                            
                              Objective To heat steel tubes to 2000 F (1093 C) in an inert atmosphere Material 0.1” (2.54mm) diameter stainless steel tube Temperature 2000 F Frequency 333 kHz Equipment • 10 kW induction heating system, equipped with a remote workhead containing… 
- 
                            induction annealing motor shaft
                            
                              Objective Annealing the end of a steel hydraulic motor shaft prior to machining Material .75” (19mm) diameter steel rod, 6” (152.4mm) long with a keyway at the end Temperature 1350 F (732 C) Frequency 359 kHz Equipment • UM-06A-UHF induction heating… 
- 
                            induction annealing aluminum tubing
                            
                              Objective Annealing aluminum fuel tank fill neck to 650 F (343 C) Material Aluminum fill neck 2.5” (63.5mm) diameter, 14” (35.5cm) long Temperature 650 F (343 C) Frequency 85 kHz Equipment • 40kW induction heating system, equipped with a remote work… 
- 
                            induction annealing brass wire
                            
                              Objective Continuously anneal a brass wire used in electric motors at a rate of 16.4 yds (15m) per minute to eliminate work hardening caused during the drawing process. Material Square copper wire 0.06” (1.7mm) dia., temperature indicating paint Tempera… 
- 
                            induction annealing aluminum lip
                            
                              Objective Annealing a 1” lip on aluminum cryogenic dewar that has been work hardened during the process of spin forming. Material Aluminum dewar, lip has a 3.24” (82.3mm) ID and is 0.05” (1.3mm) thick Temperature 800 F (427 C) Frequency 303 kHz Equi… 
- 
                            induction annealing steel wire
                            
                              Objective To heat 3” (76.2mm) from the end of the wire on a woven wire cloth 60” (1.52m) long. This prepares the wire mesh for bending in a press brake. Material Woven wire cloth (steel) made of 1/2” (12.7) diameter wire, 60” (1.52m) long. Wires are 1… 
- 
                            induction annealing copper tubing
                            
                              Objective To heat both ends of a copper tube to anneal as soft as possible 1.5” (38.1mm) from end and retain full hardness next to anneal Material 1.625” (41.275mm) dia x 24” (609.6mm) long copper tube Temperature 1500 F (815.5 C) Frequency 70 kHz E… 
- 
                            induction annealing brass crimping
                            
                              Objective To anneal a small area of an electrical contact for crimpingMaterial Brass female spade electrical contact with single transverse loop at end 0.5h(12.7mm) long, 0.25h(6.3mm) wide and 0.03h (0.8mm) thick, 1000oF (538oC)heat paintTemperature … 
- 
                            induction annealing steel shaft
                            
                              Objective Heating a steel rod to 1200F (649C) for an annealing, stress relief application Material 1.062” (26.97mm) dia type T-410 stainless steel bar 6’ (1.82m) long & 1.25” (31.75mm) dia T-416 stainless steel bar 6’ (1.82m) long Temperature 120… 